large zinc flower is normal zinc flower, according to the normal production process can produce large zinc flower, its crystal core diameter is not less than 0.2mm.

large zinc flower is normal zinc flower, according to the normal production process can produce large zinc flower, its crystal core diameter is not less than 0.2mm.

Dark spots are formed by further oxidation of white rust. The main causes of white rust are:Poor passivation, passivation film thickness is not enough or uneven; No oil on the surface or residual water on the strip surface; The surface of t···

The main reasons for zinc layer shedding are: Surface oxidation, silicon compounds, cold bound emulsion is too dirty, NOF section oxidation atmosphere and protective gas dew point is too high, air fuel ratio is unreasonable, hydrogen flow r···

What is the length of the coil?

Mainly: peeling, scratches, passivation spots, zinc particles, thick edge, air knife stripes, air knife scratches, exposed steel, inclusion, mechanical damage, poor steel base performance, wave edge, ladling bend, inappropriate size, emboss···

There are two kinds: air-cooled and water-cooled.

There are three kinds of vertical, horizontal and vertical annealing furnaces.

Product categories: General coil (CQ), structural galvanized sheet (HSLA), deep drawing hot galvanized sheet (DDQ), baking and hardening hot galvanized sheet (BH), duplex steel (DP), TRIP steel (Phase change induced plastic steel), etc.