When the hot galvanized sheet is in the humid air, especially when the air contains SiO2, CO2, NO2 and NO and other acidic substances, the surface of the galvanized layer will soon produce loose white rust.

When the hot galvanized sheet is in the humid air, especially when the air contains SiO2, CO2, NO2 and NO and other acidic substances, the surface of the galvanized layer will soon produce loose white rust.

There are three ways to test the corrosion resistance of hot-galvanized sheet: salt spray test; Wet test; Erosion test.

Chromate passivation treatment of galvanized sheet can form passivation film, its chemical reaction formula is as follows: Zn+H2GrO4-ZnGrO2=H2The trivalent chromium in solution passivation group is insoluble in water, and its chemical prope···

large zinc flower is normal zinc flower, according to the normal production process can produce large zinc flower, its crystal core diameter is not less than 0.2mm.

Dark spots are formed by further oxidation of white rust. The main causes of white rust are:Poor passivation, passivation film thickness is not enough or uneven; No oil on the surface or residual water on the strip surface; The surface of t···

The main reasons for zinc layer shedding are: Surface oxidation, silicon compounds, cold bound emulsion is too dirty, NOF section oxidation atmosphere and protective gas dew point is too high, air fuel ratio is unreasonable, hydrogen flow r···

What is the length of the coil?

Mainly: peeling, scratches, passivation spots, zinc particles, thick edge, air knife stripes, air knife scratches, exposed steel, inclusion, mechanical damage, poor steel base performance, wave edge, ladling bend, inappropriate size, emboss···